Matériaux
Chrome Tanned Leather
LeatherMay discolor unpredictably - always test first. Fumes are more irritating than veg-tan. Commonly found in upholstery and garment leather. Results vary by manufacturer.
Réglages par puissance
| Vermogen | Actie | Power (%) | Speed (mm/min) | Passes |
|---|---|---|---|---|
| 5W | engrave | 50 | 1200 | 1 |
| 5W | cut2mm | 100 | 80 | 2 |
| 10W | engrave | 40 | 1800 | 1 |
| 10W | cut2mm | 90 | 150 | 2 |
| 20W | engrave | 30 | 2500 | 1 |
| 20W | cut2mm | 80 | 250 | 1 |
| 30W | engrave | 25 | 3500 | 1 |
| 30W | cut2mm | 70 | 400 | 1 |
| 40W | engrave | 20 | 4500 | 1 |
| 40W | cut2mm | 60 | 550 | 1 |